Direct Growth of Al2O3 on Black Phosphorus by Plasma-Enhanced Atomic Layer Deposition
Related Experiment Video
Updated: Mar 3, 2026

Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures
Published on: February 8, 2018
B B Wu1,2, H M Zheng2, Y Q Ding3
1The Key Laboratory of Food Colloids and Biotechnology, Ministry of Education, School of Chemical and Material Engineering, Jiangnan University, Wuxi, 214122, Jiangsu, China.
Abstract:
Growing high-quality and uniform dielectric on black phosphorus is challenging since it is easy to react with O2 or H2O in ambient. In this work, we have directly grown Al2O3 on BP using plasma-enhanced atomic layer deposition (PEALD). The surface roughness of BP with covered Al2O3 film can reduce significantly, which is due to the removal of oxidized bubble in BP surface by oxygen plasma. It was also found there is an interfacial layer of PO x in between amorphous Al2O3 film and crystallized BP, which is verified by both X-ray photoelectron spectroscopy (XPS) and transmission electron microscopy (TEM) measurements. By increasing temperature, the PO x can be converted into fully oxidized P2O5.
More Related Videos
07:00Graphene-Assisted Quasi-van der Waals Epitaxy of AlN Film on Nano-Patterned Sapphire Substrate for Ultraviolet Light Emitting Diodes
Published on: June 25, 2020
14:16Fabrication of Schottky Diodes on Zn-polar BeMgZnO/ZnO Heterostructure Grown by Plasma-assisted Molecular Beam Epitaxy
Published on: October 23, 2018