Bond durability of contemporary adhesive systems to pulp chamber dentin
1Department of Restorative Dentistry, Faculty of Dentistry, Karadeniz Technical UniversityTrabzonTurkey.
Abstract:
Objective: The purpose of this study was to evaluate long-term bond strengths of dentin adhesive systems, which include one-step self-etch adhesive systems (Optibond All-in-one, Kerr; Adper Prompt L-POP, 3 M ESPE), a three-step etch-and-rinse adhesive (Optibond FL, Kerr) and two-step self-etch adhesive (AdheSE Bond, Ivoclar), applied to pulp chamber dentin surfaces after 12-month water storage by using microtensile bond strength (µTBS) test. Materials and methods: Dentin adhesive systems were applied to unprepared pulp chamber dentin surfaces according to manufacturer's directions, respectively (n = 5). After applying adhesive systems, composite buildups were done incrementally. Bond strengths to pulp chamber dentin surfaces were determined using µTBS test after water storage for 24 h and 12 month. Kruskal-Wallis analysis and Mann-Whitney U-test for pairwise comparisons were used to determine statistical differences in µTBS between the groups at a significance level of 5%. Results: There were no significant differences in µTBS between storage periods for tested adhesives regardless adhesive class. Conclusion: Bond durability of tested adhesive systems, including one-bottle self-etch adhesives with pulp chamber dentin surfaces, may be considered stable after 12-month water storage. Therefore, one-step self-etch, also called "user-friendly" adhesives may perform and traditional three-step etch-and-rinse adhesives in the long-term when used for bonding to pulp chamber dentin surfaces.
Related Concept Videos
Mortar Properties
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Brick Durability, Strength, and Appearance
Soundness of Cement