Homogenization Kinetics of a Nickel-based Superalloy Produced by Powder Bed Fusion Laser Sintering

Fan Zhang1, Lyle E Levine1, Andrew J Allen1

  • 1Material Measurement Laboratory, National Institute of Standards and Technology, 100 Bureau Drive, Gaithersburg, MD 20899, USA.

Scripta Materialia
|August 22, 2017
PubMed