Area-Selective Atomic Layer Deposition of SiO2 Using Acetylacetone as a Chemoselective Inhibitor in an ABC-Type Cycle

Alfredo Mameli1, Marc J M Merkx1, Bora Karasulu1

  • 1Department of Applied Physics, Eindhoven University of Technology , P.O. Box 513, 5600 MB Eindhoven, The Netherlands.

ACS Nano
|August 30, 2017
PubMed