ZnO Nanomembrane/Expanded Graphite Composite Synthesized by Atomic Layer Deposition as Binder-Free Anode for Lithium

Yalan Li1,2, Yuting Zhao2, Gaoshan Huang2

  • 1School of Energy and Power Engineering, University of Shanghai for Science and Technology , Shanghai 200093, People's Republic of China.