Novel Cyclosilazane-Type Silicon Precursor and Two-Step Plasma for Plasma-Enhanced Atomic Layer Deposition of Silicon Nitride
Related Experiment Video
Updated: Feb 14, 2026

Fabrication and Characterization of High-Q Silicon Nitride Membrane Resonators
Published on: August 8, 2025
Jae-Min Park1, Se Jin Jang2, Sang-Ick Lee2
1Department of Nanotechnology and Advanced Materials Engineering , Sejong University , 209, Neungdong-ro , Gwangjin-gu, Seoul 05006 , Republic of Korea.
Abstract:
We designed cyclosilazane-type silicon precursors and proposed a three-step plasma-enhanced atomic layer deposition (PEALD) process to prepare silicon nitride films with high quality and excellent step coverage. The cyclosilazane-type precursor, 1,3-di-isopropylamino-2,4-dimethylcyclosilazane (CSN-2), has a closed ring structure for good thermal stability and high reactivity. CSN-2 showed thermal stability up to 450 °C and a sufficient vapor pressure of 4 Torr at 60 °C. The energy for the chemisorption of CSN-2 on the undercoordinated silicon nitride surface as calculated by density functional theory method was -7.38 eV. The PEALD process window was between 200 and 500 °C, with a growth rate of 0.43 Å/cycle. The best film quality was obtained at 500 °C, with hydrogen impurity of ∼7 atom %, oxygen impurity less than 2 atom %, low wet etching rate, and excellent step coverage of ∼95%. At 300 °C and lower temperatures, the wet etching rate was high especially at the lower sidewall of the trench pattern. We introduced the three-step PEALD process to improve the film quality and the step coverage on the lower sidewall. The sequence of the three-step PEALD process consists of the CSN-2 feeding step, the NH3/N2 plasma step, and the N2 plasma step. The H radicals in NH3/N2 plasma efficiently remove the ligands from the precursor, and the N2 plasma after the NH3 plasma removes the surface hydrogen atoms to activate the adsorption of the precursor. The films deposited at 300 °C using the novel precursor and the three-step PEALD process showed a significantly improved step coverage of ∼95% and an excellent wet etching resistance at the lower sidewall, which is only twice as high as that of the blanket film prepared by low-pressure chemical vapor deposition.
More Related Videos
05:02Growth of Gold Dendritic Nanoforests on Titanium Nitride-coated Silicon Substrates
Published on: June 3, 2019
08:18Synthesis and Characterization of High c-axis ZnO Thin Film by Plasma Enhanced Chemical Vapor Deposition System and its UV Photodetector Application
Published on: October 3, 2015
Related Concept Videos
Inductively Coupled Plasma Atomic Emission Spectroscopy: Principle
The ions and electrons produced interact with the fluctuating magnetic field created by a water-cooled...
Inductively Coupled Plasma Atomic Emission Spectroscopy: Instrumentation
There are three main types of inductively coupled plasma atomic emission spectroscopy (ICP-AES) instruments: sequential, simultaneous multichannel, and Fourier transform instruments, with the latter being less commonly used....
Composition of Blood Plasma
Enlargement of the Plasma Membrane
Plasma Membrane in Bacteria and Archaea
Drug Distribution: Plasma Protein Binding