Mapping the Galvanic Corrosion of Three Coupled Metal Alloys Using Coupled Multielectrode Array: Influence of

Hong Ju1, JinZhuo Duan2, Yuanfeng Yang3

  • 1College of Mechanical and Electronic Engineering, China University of Petroleum, Qingdao 266580, China. juhong@upc.edu.cn.

Related Concept Videos

Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
28.5K
Voltaic/Galvanic Cells02:47

Voltaic/Galvanic Cells

Spontaneous Chemical Reactions
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
63.8K
Spin–Spin Coupling: Two-Bond Coupling (Geminal Coupling)01:20

Spin–Spin Coupling: Two-Bond Coupling (Geminal Coupling)

Two NMR-active nuclei bonded to a central atom can be involved in geminal or two-bond coupling. Geminal coupling is commonly seen between diastereotopic protons in chiral molecules and unsymmetrical alkenes, among others.
The central atom need not be NMR-active because its electrons are affected by the electron polarization of the spin-active atoms. However, spin information is transmitted less effectively than in one-bond coupling, and 2J values are usually weaker than 1J values. The energy of...
1.7K
Spin–Spin Coupling: Three-Bond Coupling (Vicinal Coupling)01:22

Spin–Spin Coupling: Three-Bond Coupling (Vicinal Coupling)

Vicinal or three-bond coupling is commonly observed between protons attached to adjacent carbons. Here, nuclear spin information is primarily transferred via electron spin interactions between adjacent C‑H bond orbitals. This generally favors the antiparallel arrangement of spins, so 3J values are usually positive.
The extent of coupling depends on the C‑C bond length, the two H‑C‑C angles, any electron-withdrawing substituents, and the dihedral angle between the involved orbitals. The...
1.5K
G-protein Coupled Receptors01:21

G-protein Coupled Receptors

G-protein coupled receptors are ligand binding receptors that indirectly affect changes in the cell. The actual receptor is a single polypeptide that transverses the cell membrane seven times creating intracellular and extracellular loops. The extracellular loops create a ligand specific pocket which binds to neurotransmitters or hormones. The intracellular loops holds onto the G-protein.
132.2K
Spin–Spin Coupling: One-Bond Coupling01:17

Spin–Spin Coupling: One-Bond Coupling

Coupling interactions are strongest between NMR-active nuclei bonded to each other, where spin information can be transmitted directly through the pair of bonding electrons. While nuclei polarize their electrons to the opposite spins, the bonding electron pair has opposite spins. Configurations with antiparallel nuclear spins are expected to be lower in energy. When coupling makes antiparallel states more favorable, J is considered to have a positive value. The one-bond coupling constant, 1J,...
1.5K