Fast formation of a supramolecular ion gel/solvoplastic elastomer with excellent stretchability
Shishun Bai1, Xin Wang1, Jaana Vapaavuori2
1School of Materials Science and Engineering, Energy Polymer Research Center, Southwest Petroleum University, 8 Xindu Avenue, Chengdu, Sichuan 610500, China.
Abstract:
This study describes a simple yet efficient approach for the preparation of an ionic gel that is also elastomeric in its solid-state bulk form. A series of poly(2-(diethylamino)ethyl methacrylate-co-lauryl methacrylate) P(DMAEMA-co-LMA) copolymers were synthesized first by radical polymerization. Quaternization of the PDMAEMA component in tetrahydrofuran enables the formation of supramolecular network, giving rise to an ion gel. An elastomer with an elongation at break of over 600% was obtained from the gel. The elastomer, connected by supramolecular ionic cross-links, is solvoplastic in certain solvents. The simple yet efficient approach of the formation of ion-gel and the dried elastomer allows fast preparation of both gel-like and solid-state elastic materials for various applications where recyclability is required.
Related Concept Videos
Formation of Complex Ions
Microsoft Excel: Plotting Mean, SD, and SE
First, calculate the mean, SD, and SE of your data. The mean is obtained using the formula `=AVERAGE(range)`, while SD can be calculated with `=STDEV.P(range)` for a population or `=STDEV.S(range)` for a sample. SE is calculated as `=SD/SQRT(n)`, where `n` is the sample size.
To plot these values, use a bar...
Microsoft Excel: Student's t-Test
To conduct a t-test in Excel, use the T.TEST function or the "Data...
Common Ion Effect
Microsoft Excel: Pearson's Correlation
Microsoft Excel: Regression Analysis
To perform regression...