Abstract:
The aim of this paper is to explore the watertightness behaviour for high pressure applications using Multi Jet Fusion technology and polyamide 12 as a material. We report an efficient solution for manufacturing functional prototypes and final parts for water pressure applications and provide manufacturing rules for engineers in the pressurized product development process for up to 10 MPa of nominal pressure. The research findings show manufacturers the possibility of using additive manufacturing as an alternative to traditional manufacturing. Water leakage was studied using different printing orientations and wall thicknesses for a range of pressure values. An industrial ball valve was printed and validated with the ISO 9393 standard as also meeting tolerance requirements. This paper is a pioneering approach to the additive manufacturing of high-performance fluid handling components. This approach solves the problem of leakage caused by porosity in additive manufacturing technologies.
Related Concept Videos
Free Jet
Nuclear Fusion
A helium nucleus has a mass that is 0.7% less than that of four hydrogen nuclei; this lost mass is converted into energy during the fusion. This reaction produces about...
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Steel Manufacturing
During this smelting process, limestone plays a crucial role by forming slag. Slag captures impurities within the molten iron, such...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete