A simple and versatile machine for creep testing at low loads (6-300 N) and on miniaturized specimens: Application to

N T B N Koundinya1, Nandha Kumar E1, Niraj Chawake1

  • 1Department of Metallurgical and Materials Engineering, Indian Institute of Technology Madras, Chennai 600 036, India.

Related Concept Videos

Creep in Concrete01:22

Creep in Concrete

Creep refers to the time-dependent increase in strain under a sustained load, excluding other time-dependent deformations associated with shrinkage, swelling, and thermal expansion in concrete. The primary mechanism behind creep involves the loss of physically adsorbed water from the calcium silicate hydrate within the hydrated cement paste. This process is further exacerbated by concrete's non-linear stress-strain relationship, microcrack development in the interfacial transition zone, and...
1.3K
Factors Affecting Creep01:28

Factors Affecting Creep

In normal-weight aggregate concrete, the hardened cement paste is the primary contributor to creep, whereas the aggregates, being stiffer than the cement paste, are more resilient to stress-induced deformation. The stiffness of the aggregates is defined by their modulus of elasticity, and the more voluminous they are in the concrete, the less it will creep.
Further, the water/cement ratio is critical, as a lower ratio increases concrete strength, thus reducing creep. The strength of the...
457
Effects of Creep01:25

Effects of Creep

Creep in concrete, the gradual deformation under prolonged stress, significantly impacts the integrity of structures. For reinforced concrete beams, it can be a vital design consideration, as it increases deflection, sometimes necessitating additional design measures. In columns, especially slender ones under eccentric loads, creep can cause buckling, compromising their stability. However, creep can be beneficial in indeterminate structures by mitigating stresses that arise from shrinkage,...
449
Machines01:19

Machines

Machines are complex structures consisting of movable, pin-connected multi-force members that work together to transmit forces. One example of a machine is the cutting plier, which is used to cut wires by applying forces to its handles. When equal and opposite forces are exerted on the handles of the cutting plier, they cause the cutting edges to come together and apply equal and opposite reaction forces on the wire, which are greater than the applied forces.
A free-body diagram of the...
579
Machines: Problem Solving II01:30

Machines: Problem Solving II

Machines are complex structures consisting of movable, pin-connected multi-force members that work together to transmit forces. Consider a lifting tong carrying a 100 kg load. It comprises movable sections DAF and CBG linked together with member AB.
668
Machines: Problem Solving I01:22

Machines: Problem Solving I

A toggle clamp is a mechanical device commonly used for holding and clamping objects in various applications, such as woodworking, metalworking, and assembly operations. Consider a toggle clamp subjected to a force of 200 N at the handle. The vertical clamping force can be calculated, provided the dimensions of the toggle clamp are known.
The toggle clamp system is a machine structure consisting of movable, pin-connected multi-force members that form a stabilized system to transmit forces. The...
714