Analysis of Electrical and Nano-Mechanical Properties of Cu-Fe Thin Foil Using Dynamic Nanoindentation

Bo Kyeong Kang1, Youl Baik1, Yong Choi1

  • 1Department of Materials Science and Engineering, Dankook University, Cheonan, Chungnam, 31116, Republic of Korea.

Related Concept Videos

Sources and Properties of Electric Charge01:15

Sources and Properties of Electric Charge

All objects we see around us consist of atoms, which combine to form molecules. The lightest element in the universe is hydrogen, and a hydrogen atom consists of a positively charged proton and a negatively charged electron. The magnitude of charge that a proton and an electron carry are the same, and it is the fundamental unit of charge. In SI units, it is 1.602 times 10-19 coulomb.
Most atoms additionally constitute another fundamental particle, the neutron. It carries no electrical charge. A...
12.7K
Properties of Electric Field Lines01:25

Properties of Electric Field Lines

The definition of electric field lines greatly eases the visualization of electric fields, a vector field, especially in the presence of many charges. The one-to-one correspondence between the electric field and the electric field lines necessitates that the field lines follow some rules.
For one, the electric field of a positive charge must originate from it. That is because its electric field points away from it. Moreover, since the magnitude of the field asymptotes to zero at infinity, the...
9.6K
1° Amines to Diazonium or Aryldiazonium Salts: Diazotization with NaNO2 Mechanism01:37

1° Amines to Diazonium or Aryldiazonium Salts: Diazotization with NaNO2 Mechanism

Nitrous acid is a relatively weak and unstable acid prepared in situ by the reaction of sodium nitrite and cold, dilute hydrochloric acid. In an acidic solution, the nitrous acid undergoes protonation when it loses water to form a nitrosonium ion—an electrophile. Nitrous acid reacts with primary amines to give diazonium salts. The reaction is called diazotization of primary amines.
4.9K
Physical and Chemical Properties of Matter02:57

Physical and Chemical Properties of Matter

The characteristics that enable us to distinguish one substance from another are called properties.
166.4K
Properties of Transition Metals02:58

Properties of Transition Metals

Transition metals are defined as those elements that have partially filled d orbitals. As shown in Figure 1, the d-block elements in groups 3–12 are transition elements. The f-block elements, also called inner transition metals (the lanthanides and actinides), also meet this criterion because the d orbital is partially occupied before the f orbitals.
29.8K
Dynamic Equilibrium02:20

Dynamic Equilibrium

A reversible chemical reaction represents a chemical process that proceeds in both forward (left to right) and reverse (right to left) directions. When the rates of the forward and reverse reactions are equal, the concentrations of the reactant and product species remain constant over time and the system is at equilibrium. A special double arrow is used to emphasize the reversible nature of the reaction. The relative concentrations of reactants and products in equilibrium systems vary greatly;...
62.7K