Ti2Nb10O29 microspheres coated with ultrathin N-doped carbon layers by atomic layer deposition for enhanced lithium
Gengping Wan1, Liang Yang, Shaohua Shi
1Key Laboratory of Advanced Materials of Tropical Island Resources (Hainan University), Ministry of Education, Haikou 570228, China. wangguizhen0@hotmail.com.
Abstract:
A novel design of 3D porous Ti2Nb10O29 microspheres coated with ultrathin N-doped carbon layers, which can improve electron/ion transport, shows remarkable high-rate capacity (267 mA h g-1 at 10C and 199 mA h g-1 at 40C) and stable cycle lives with a high capacity retention rate of 90.2% after 500 cycles.
Related Concept Videos
Layers of the Epidermis
Stratum Basale
Stratum basale, also known as the stratum germinativum, is the deepest layer of the epidermis. It is composed of a single layer of actively dividing cells called basal cells or basal keratinocytes. These cells constantly undergo cell division to replenish the upper layers of the epidermis. Additionally, melanocytes, which...
Thematic Layering in GIS
Layers of the Heart Wall
The myocardium, the thickest layer, consists of cardiac muscle cells interconnected by intercalated discs and crisscrossing connective tissue fibers. These muscle fibers contract...
Boundary Layer Characteristics
Thin-Layer Chromatography (TLC): Overview
To begin the analysis, a mixture of compounds is spotted on the starting line on the TLC plate using a thin capillary. The bottom of the...
Layers of Connective Tissue Proper