Finite element simulation based-on atomic force microscopy and nanoindentation for spruce wood microstructure

David Torres-Torres1, Jesús A Torres2, Alejandra García-García3

  • 1Laboratorio de Análisis de Integridad en Desempeño Mecánico de Dispositivos y Materiales Avanzados, CIMAV, S.C. Unidad Monterrey, Apodaca, Nuevo Léon, Mexico.

Related Concept Videos

Atomic Force Microscopy01:08

Atomic Force Microscopy

Atomic force microscopy (AFM) is a type of scanning probe microscopy that can analyze topographic details of various specimens like ceramics, glass, polymers, and biological samples. AFM offers over 1000 times more resolution than the optical imaging system. Images generated from AFM are three-dimensional surface profiles, offering an advantage over the flat, two-dimensional images from other imaging techniques.
The AFM Probe
The probe is regarded as the heart of any AFM setup and comprises the...
4.5K
Elements and Compounds01:27

Elements and Compounds

Pure substances consist of only one type of matter. A pure substance can be an element or a compound. An element consists of only one type of atom, while a compound consists of two or more types of atoms held together by a chemical bond.
Elements
Elements are classified as atomic or molecular based on the nature of their basic units. They are unique forms of matter with specific chemical and physical properties that cannot break down into smaller substances by ordinary chemical reactions. There...
104.6K
Classification of Elements and Compounds02:54

Classification of Elements and Compounds

Pure substances consist of only one type of matter. A pure substance can be an element or a compound. An element consists of only one type of atom, while a compound consists of two or more types of atoms held together by a chemical bond. Elements are classified as atomic or molecular based on the nature of their basic units.
Compounds are pure substances composed of two or more elements in fixed, definite proportions. Compounds are classified as ionic or molecular (covalent) based on the bonds...
73.1K
Periodic Classification of the Elements04:00

Periodic Classification of the Elements

The periodic table arranges atoms based on increasing atomic number so that elements with the same chemical properties recur periodically. When their electron configurations are added to the table, a periodic recurrence of similar electron configurations in the outer shells of these elements is observed. Because they are in the outer shells of an atom, valence electrons play the most important role in chemical reactions. The outer electrons have the highest energy of the electrons in an atom...
59.0K
Atomic Structure01:33

Atomic Structure

Overview
209.4K
Atomic Mass01:52

Atomic Mass

Atoms — and the protons, neutrons, and electrons that compose them — are extremely small. For example, a carbon atom weighs less than 2 × 10−23 g. When describing the properties of tiny objects such as atoms, we use appropriately small units of measure, such as the atomic mass unit (amu). The amu was originally defined based on hydrogen, the lightest element, then later in terms of oxygen. Since 1961, it has been defined with regard to the most abundant isotope of carbon, atoms of which...
70.1K