Plasma-Enhanced Atomic Layer Deposition of TiAlN: Compositional and Optoelectronic Tunability
Related Experiment Video
Updated: Jan 28, 2026

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model
Published on: May 23, 2018
Nari Jeon, Ian Lightcap1, David J Mandia
1Center for Sustainable Energy at Notre Dame , University of Notre Dame , Notre Dame , Indiana 46556 , United States.
Abstract:
Titanium nitride (TiN) is a unique refractory plasmonic material, the nanocomposites and alloys of which provide further opportunities to tailor its optical and photonic properties. We prepare TiAlN films of continuously variable compositions through the systematic variation of TiN versus AlN cycle ratio in plasma-enhanced atomic layer deposition (PEALD) and investigate the resulting thin-film composition, crystallinity, and optical properties. The resulting properties of TiAlN films are not simple linear combinations of the TiN and AlN films, which exhibit distinct metallic and dielectric properties, but instead are dramatically influenced by the local chemical environment of neighboring constituents. In situ spectroscopic ellipsometry further enables measurement of the varying optical properties of TiAlN films, which evolve over 10 s of nm of film thickness. The tunable optoelectronic properties of TiAlN films enable durable coatings of variable electrical resistance as well as high-temperature diffusion barriers and optical coatings with application to selective solar absorbers and emitters.
Related Concept Videos
Composition of Blood Plasma
Classifying Matter by Composition
According to its composition, the matter can be classified into two broad categories — pure substances and mixtures.
A pure substance is a form of matter that has a constant composition throughout with uniform properties. For example, any sample of sucrose has the same composition and same physical properties, such as melting point, color, and sweetness, regardless of the source from which it is isolated.
A mixture is composed of two or...
Inductively Coupled Plasma Atomic Emission Spectroscopy: Principle
The ions and electrons produced interact with the fluctuating magnetic field created by a water-cooled...
Inductively Coupled Plasma Atomic Emission Spectroscopy: Instrumentation
There are three main types of inductively coupled plasma atomic emission spectroscopy (ICP-AES) instruments: sequential, simultaneous multichannel, and Fourier transform instruments, with the latter being less commonly used....
Atomic Structure
Atomic Mass