Marginal fit of metal-ceramic crowns fabricated by using a casting and two selective laser melting processes before
Min-Ho Hong1, Bong Ki Min2, Du-Hyeong Lee3
1Postdoctoral Researcher, Institute for Biomaterials Research and Development, Kyungpook National University, Daegu, Republic of Korea.
Statement Of Problem:
Few studies have investigated changes in the marginal fit of metal-ceramic restorations fabricated by selective laser melting (SLM) techniques after the application of veneering ceramic.
Purpose:
The purpose of this in vitro study was to evaluate the marginal fit (silicone replica technique) and internal porosity (cross-section analysis) of cobalt-chromium (Co-Cr) alloy metal crowns prepared by using 2 SLM processes together with a casting technique before and after ceramic veneering.
Material And Methods:
Cast single Co-Cr crowns and SLM-processed crowns with large (SLML) or small (SLMS) porosity were prepared (n=20/group), and half were subjected to ceramic veneering. On a single Co-Cr master die, the marginal discrepancy (MD) and absolute marginal discrepancy (AMD) of the crowns were measured by using the silicone replica technique, in which each replica was cut into 4 sections before and after ceramic veneering (n=10 for each subgroup). After marginal fit measurements, each metal coping was cross-sectioned into 4 parts, and 5 rectangular optical microscope images were acquired on both outer corners of each quarter. The porosity was then calculated as the ratio of the black-to-white pixels on the binarized images. The data were analyzed by 2-way ANOVA and the post hoc test (Tukey or Student t test) (α=.05).
Results:
Before ceramic veneering, the 2 SLM groups showed significantly larger MDs than the casting group (56.4 ±10.4 μm) (P<.05). A significant increase in MD after ceramic veneering was detected only in the SLML group (P<.001). The AMD values showed a similar trend with MD values. The 2 SLM groups (in particular, SLML) showed a significantly higher amount of porosity than the casting group before ceramic veneering (P<.001). Only the SLML group showed a significant decrease in the amount of porosity after ceramic veneering (P<.001).
Conclusions:
Within the limitations of this in vitro study, large internal porosity within the SLM-fabricated Co-Cr metal copings affected the marginal fit of the metal-ceramic crowns. However, all the MD values of the 3 groups were lower than the acceptable range even after the application of veneering ceramic.
More Related Videos
06:53Additive Manufacturing of Functionally Graded Ceramic Materials by Stereolithography
Published on: January 25, 2019
08:29Multi-material Ceramic-Based Components – Additive Manufacturing of Black-and-white Zirconia Components by Thermoplastic 3D-Printing (CerAM - T3DP)
Published on: January 7, 2019
Related Concept Videos
Crown Ethers
Phase Transitions: Melting and Freezing
Metallic Solids
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and malleability....
Alkali Metals
Table 1: Properties of the alkali metals
Induced-fit Model
Enzymes exhibit substrate specificity, meaning that they can only bind to certain substrates. This is mainly determined by the shape and chemical...
Inclusive Fitness