Evaluation of Shear Bond Strength of Three Different Acrylic Resin and Artificial Denture Teeth with and without
Navleen Dandiwal1, Sandeep Kumar2, Shashikala Jain2
1Department of Prosthodontics, Surendera Dental College & Research Institute Sriganganagar, Rajasthan, India, Mobile: 9521497105,
Aim:
To compare and evaluate the shear bond strength of the tooth-denture base junction when three different commercially available acrylic resin base bonded to acrylic teeth with and without application of methyl methacrylate monomer on ridge lap area.
Materials And Methods:
A three-stepped cylindrical shaped die was customized. Sixty samples were fabricated with heat cure and self-cure acrylic resin with and without monomer application. A total of 60 samples were divided into three groups and six subgroups. • Group A-Twenty samples of Trevlon-HI heat-activated acrylic resin. • Subgroup A1-Ten samples of acrylic teeth bonded with Trevlon-HI heat-activated acrylic resin with the application of monomer on ridge lap area. • Subgroup A2-Ten samples of acrylic teeth bonded with Trevlon-HI heat-activated acrylic resin without application of monomer on ridge lap area. • Group B-Twenty samples of Trevalon heat-activated acrylic resin. • Subgroup B1-Ten samples of acrylic teeth bonded with Trevlon heat-activated acrylic resin with the application of monomer on ridge lap area. • Subgroup B2-Ten samples of acrylic teeth bonded with Trevlon heat-activated acrylic resin without application of monomer on ridge lap area. • Group C-Twenty samples of Trevlon-RR self-activated acrylic resin. • Subgroup C1-Ten samples of acrylic teeth bonded with Trevlon-RR self-activated acrylic resin with the application of monomer on ridge lap area. • Subgroup C2-Ten samples of acrylic teeth bonded with Trevlon-RR self-activated acrylic resin without monomer application on ridge lap area.
Results:
Samples obtained from high impact heat cure acrylic resin with monomer application shows higher bond strength when tested under the universal testing machine.
Conclusion:
With and without monomer application on high impact polymethylmethacrylate (PMMA) resin and Heat cured resin it was found that high impact shows better bond strength. Trevlon HI monomer shows a greater increase in strength due to the presence of cross-linking agents.
Clinical Significance:
The incorporation of mechanical surface treatments followed by monomer application significantly influences the bonding between denture teeth and denture base resin.
Related Concept Videos
Bonding and Strength of Aggregate
Peptide Bonds
Bond Energies and Bond Lengths
Ionic Bonds
When atoms gain or lose electrons to achieve a more stable electron configuration they form ions. Ionic bonds are electrostatic attractions between ions with opposite charges. Ionic compounds are rigid and brittle when solid and may dissociate into their constituent ions in water. Covalent compounds, by contrast, remain intact unless a chemical reaction breaks them.
Opposing Charges Hold Ions Together in Ionic Compounds
Ionic bonds are reversible electrostatic interactions between ions...
Teeth
In the bud stage, the tooth germ (an aggregation of cells) starts to form in the developing jawbone. During the cap stage, the tooth germ differentiates into enamel organ, dental papilla, and dental sac, which will later develop into the tooth's enamel, dentin...
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...