Bond Properties of Steel Bar in Concrete under Water Environment

Li Song1, Fulai Qu2, Guirong Liu2

  • 1Yellow River Institute of Hydraulic Research, Zhengzhou 450003, China.

Related Concept Videos

Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
456
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
917
Reinforcements in Concrete01:25

Reinforcements in Concrete

Reinforced concrete is a composite material used extensively in construction, combining the compressive strength of concrete with the tensile strength of steel. This synergy is essential as concrete, while excellent at resisting compression, is weak under tension. Steel bars, or rebars, are embedded in the concrete to handle these tensile forces. The choice of steel is strategic; it shares a similar coefficient of thermal expansion with concrete, which ensures uniformity in response to...
387
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
314
Tensile Strength Considerations of Concrete01:16

Tensile Strength Considerations of Concrete

Considering the tensile strength of concrete involves recognizing that the theoretical strength of cement paste can be up to a thousand times higher than what is observed in practical applications. This significant discrepancy is largely attributed to the presence of microscopic cracks within the concrete. These cracks tend to amplify stress at their tips when a load is applied, a phenomenon explained by Griffith's theory of brittle fracture.
The dimensions and shape of a concrete specimen...
451
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
407