Systematic review and meta-analysis of welding procedures in one-piece cast implant-supported frameworks

Jéssica Marcela de Luna Gomes1, Sandra Lúcia Dantas de Moraes2, Cleidiel Aparecido Araujo Lemos1

  • 1Universidade Estadual Paulista - Unesp, Araçatuba Dental School, Department of Dental Materials and Prosthodontics, Araçatuba, SP, Brazil.