New Epoxy Thermosets Derived from Clove Oil Prepared by Epoxy-Amine Curing

David Santiago1, Dailyn Guzmán1, Xavier Ramis2

  • 1Eurecat-Chemical Technology Unit, c/Marcel lí Domingo 2, Edif. N5, 43007 Tarragona, Spain.

Polymers
|January 2, 2020
PubMed

Related Concept Videos

Preparation of Epoxides03:00

Preparation of Epoxides

Overview
Epoxides result from alkene oxidation, which can be achieved by a) air, b) peroxy acids, c) hypochlorous acids, and d) halohydrin cyclization.
Epoxidation with Peroxy Acids
Epoxidation of alkenes via oxidation with peroxy acids involves the conversion of a carbon–carbon double bond to an epoxide using the oxidizing agent meta-chloroperoxybenzoic acid, commonly known as MCPBA. Since the O–O bond of peroxy acids is very weak, the addition of electrophilic oxygen of peroxy acids to...
9.0K
Base-Catalyzed Ring-Opening of Epoxides02:26

Base-Catalyzed Ring-Opening of Epoxides

Due to their highly strained structures, epoxides can readily undergo ring-opening reactions through nucleophilic substitution, either in the presence of an acid or a base. The nucleophilic substitution reactions in the presence of acid are called acid-catalyzed ring-opening reactions, and nucleophilic substitution reactions in the presence of a base are called base-catalyzed ring-opening reactions. Epoxides undergo base-catalyzed ring-opening reactions in the presence of a strong nucleophile...
9.9K
Acid-Catalyzed Ring-Opening of Epoxides02:24

Acid-Catalyzed Ring-Opening of Epoxides

Epoxides that are three-membered ring systems are more reactive than other cyclic and acyclic ethers. The high reactivity of epoxides originates from the strain present in the ring. This ring strain acts as a driving force for epoxides to undergo ring-opening reactions either with halogen acids or weak nucleophiles in the presence of mild acid. The acid catalyst converts the epoxide oxygen, a poor leaving group, into an oxonium ion, a better leaving group, making the reaction feasible. The...
8.5K
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
317
Accelerated Curing of Concrete01:25

Accelerated Curing of Concrete

Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
400
Curing Methods01:26

Curing Methods

Concrete members with a small surface-to-volume ratio are cured by oiling and moistening the forms before casting the concrete member. These forms can be left in place for a prolonged period to prevent moisture loss, and can be wetted if made of a material suitable for wetting. If the forms are removed early, the concrete member is moistened and covered with polythene sheets to maintain moisture. For large horizontal concrete surfaces exposed to dry weather, a temporary covering is suspended...
240