Microstructure and Creep Properties of Boron- and Zirconium-Containing Cobalt-based Superalloys
Peter J Bocchini1, Chantal K Sudbrack2, Ronald D Noebe2
1Department of Materials Science and Engineering, Northwestern University, 2220 Campus Drive, Evanston, Illinois 60208-3108, USA.
Abstract:
The effects of micro-additions of boron and zirconium on grain-boundary (GB) structure and strength in polycrystalline γ(f.c.c.) plus γ'(L12) strengthened Co-9.5Al-7.5W-X at. % alloys (X = 0-Temary, 0.05B, 0.01B, 0.05Zr, and 0.005B-0.05Zr at. %) are studied. Creep tests performed at 850 °C demonstrate that GB strength and cohesion limit the creep resistance and ductility of the ternary B- and Zr-free alloy due to intergranular fracture. Alloys with 0.05B and 0.005B-0.05Zr both exhibit improved creep strength due to enhanced GB cohesion, compared to the baseline ternary Co-9.5Al-7.5W alloy, but alloys containing 0.01B or 0.05Zr additions displayed no benefit. Atom-probe tomography is utilized to measure GB segregation, where B and Zr are demonstrated to segregate at GBs. A Gibbsian interfacial excess of 5.57 ± 1.04 atoms nm-2 was found for B at a GB in the 0.01B alloy and 2.88 ± 0.81 and 2.40 ± 0.84 atoms nm-2 for B and Zr, respectively, for the 0.005B-0.05Zr alloy. The GBs in the highest B-containing (0.05B) alloy exhibit micrometer-sized boride precipitates with adjacent precipitate denuded-zones (PDZs), whereas secondary precipitation at the GBs is not present in the other four alloys. The 0.05B alloy has the smallest room temperature yield strength, by 6 %, which is attributed to the PDZs, but it exhibits the largest increase in creep strength (with an ~2.5 order of magnitude decrease in the minimum strain rate for a given stress at 850 °C) over the baseline Co-9.5Al-7.5W alloy.
Related Concept Videos
Factors Affecting Creep
Further, the water/cement ratio is critical, as a lower ratio increases concrete strength, thus reducing creep. The strength of the...
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as...
Creep in Concrete
Effects of Creep
Fiber Reinforced Concrete