Related Experiment Video
Updated: Dec 27, 2025

Synthesis of Platinum-nickel Nanowires and Optimization for Oxygen Reduction Performance
Published on: April 27, 2018
Atomic layer deposition of Pd nanoparticles on self-supported carbon-Ni/NiO-Pd nanofiber electrodes for
Ahmed Barhoum1, Heba H El-Maghrabi2, Igor Iatsunskyi3
1Chemistry Department, Faculty of Science, Helwan University, Ain Helwan, Cairo 11795, Egypt; Institut Européen des Membranes (IEM), UMR-5635, Univ Montpellier, ENSCM, CNRS, Place Eugène Bataillon, 34095 Montpellier, France.
Abstract:
The most critical challenge in hydrogen fuel production is to develop efficient, eco-friendly, low-cost electrocatalysts for water splitting. In this study, self-supported carbon nanofiber (CNF) electrodes decorated with nickel/nickel oxide (Ni/NiO) and palladium (Pd) nanoparticles (NPs) were prepared by combining electrospinning, peroxidation, and thermal carbonation with atomic layer deposition (ALD), and then employed for hydrogen evolution and oxygen evolution reactions (HER/OER). The best CNF-Ni/NiO-Pd electrode displayed the lowest overpotential (63 mV and 1.6 V at j = 10 mA cm-2), a remarkably small Tafel slope (72 and 272 mV dec-1), and consequent exchange current density (1.15 and 22.4 mA cm-2) during HER and OER, respectively. The high chemical stability and improved electrocatalytic performance of the prepared electrodes can be explained by CNF functionalization via Ni/NiO NP encapsulation, the formation of graphitic layers that cover and protect the Ni/NiO NPs from corrosion, and ALD of Pd NPs at the surface of the self-supported CNF-Ni/NiO electrodes.
More Related Videos
08:40Synthesis of Metal Nanoparticles Supported on Carbon Nanotube with Doped Co and N Atoms and its Catalytic Applications in Hydrogen Production
Published on: December 6, 2021
10:57Synthesis and Performance Characterizations of Transition Metal Single Atom Catalyst for Electrochemical CO2 Reduction
Published on: April 10, 2018