Heat Capacities of Polyethylene IV. High Molecular Weight Linear Polyethylene
1Institute for Materials Research, National Bureau of Standards, Washington, D.C. 20234.
Abstract:
A high molecular weight linear polyethylene sample has been studied by adiabatic calorimetry from 10 to 380 K. Two broad temperature regions of unusual spontaneous temperature drift have been observed. The phenomena occurring around 240 K are similar to that observed in other polyethylene samples studied in this series, and are presumed to be caused by the relaxational processes in the amorphous phase. The weak exothermic behavior occurring around 160 K is presumed to be caused by the stabilization of the quenched sample.
Related Concept Videos
Polymer Classification: Architecture
Free-Radical Chain Reaction and Polymerization of Alkenes
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Polymers: Molecular Weight Distribution
Polymer Classification: Stereospecificity