Sabra Jaâfoura1, Amira Kikly2, Saida Sahtout2
1Department of Dental Biomaterials, ABCDF Laboratory, Faculty of Dental Medicine, University of Monastir, Avicenne Avenue, Monastir 5000, Tunisia.
Introduction:
This in vitro study compared the shear strength of three composite resin systems to fluorosed and normal dentin.
Methods:
Silorane FiltekTM P90, FiltekTMZ250 XT in combination with the adhesive system AdperTM Single bond 2, and Amelogen® Plus in association with Peak Universal Bond® were tested. Fifteen normal and 15 fluorosed dentine disks were prepared per material. The shear bond strength test was performed using a universal machine.
Results:
One-way ANOVA revealed significant differences in bond strength between the tested composite resins. All tested materials had significantly different adhesion at the fluorosed and the nonfluorosed interface. FiltekTM Z250 XT and Silorane had lower adhesion values to fluorosed than to normal dentin. In contrast, Amelogen® Plus presented a better average resistance at the fluorosed interface.
Conclusion:
Amelogen® Plus presented a better average shear bond strength on the fluorosed dentine. FiltekTMZ250 XT showed the best adhesion forces and shear bond strength with sound dentine. Further studies are needed to better understand the sealing of these systems.
More Related Videos
05:30Roughness Impact of Piezoelectric Dental Scaler on Two Distinct Flowable Composite Filling Materials
Published on: January 10, 2025
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024