Related Experiment Video
Updated: Dec 18, 2025

Fabricating Metamaterials Using the Fiber Drawing Method
Published on: October 18, 2012
Tailoring the Diameters of Electro-Mechanically Spun Fibers by Controlling Their Deborah Numbers
Domingo R Flores-Hernandez1, Braulio Cardenas-Benitez1, Sergio O Martinez-Chapa1
1Escuela de Ingeniería y Ciencias, Tecnologico de Monterrey, Ave. Eugenio Garza Sada 2501, Monterrey 64849, NL, Mexico.
Abstract:
Polymer solutions with different concentrations of SU-8 2002/poly(ethylene) glycol/tetrabutyl ammonium tetrafluoroborate (SU-8/PEO/TBATFB) were electrospun in a low-voltage near-field electrospinning platform (LVNFES) at different velocities. Their diameters were related to the concentration contents as well as to their Deborah (De) numbers, which describes the elasticity of the polymer solution under determined operating conditions. We found a direct correlation between the concentration of PEO/TBATFB, the De and the diameter of the fibers. Fibers with diameters as thin as 465 nm can be achieved for De ≈ 1.
More Related Videos
07:38Microfluidic Fabrication of Polymeric and Biohybrid Fibers with Predesigned Size and Shape
Published on: January 8, 2014
12:28Melt Electrospinning Writing of Three-dimensional Poly(ε-caprolactone) Scaffolds with Controllable Morphologies for Tissue Engineering Applications
Published on: December 23, 2017