Morphology and Dissolution Rate of Wear Debris from Silicon Nitride Coatings
Maria Pettersson1, Charlotte Skjöldebrand1, Luimar Filho1
1Materials in Medicine Group, Division of Applied Materials Science, Department of Engineering Sciences, Uppsala University, Lägerhyddsvägen 1, 752 37 Uppsala, Sweden.
Abstract:
Silicon nitride (SiN) coatings have recently been introduced as a potential material for joint implant bearing surfaces, but there is no data on wear debris morphology nor their dissolution rate, something that could play a central role to implant longevity. In this study, wear debris was generated in a ball-on-disc setup in simulated body fluid. After serum digestion the debris was analyzed with scanning electron microscopy and energy-dispersive X-ray spectroscopy. The particle dissolution rate was evaluated using inductively coupled plasma techniques, on model SiN particles. The wear debris from SiN coatings was found to be round, in the nm range and formed agglomerates in the submicrometer to micrometer range. Model particles dissolved in simulated body fluid at a rate of: c(t) = 39.45[1 - exp(-1.11 × 10-6t)], where [c(t)] = mg/L and [t] = s. This study can be used as a preliminary prediction of size, shape, and dissolution rate of wear debris from SiN coatings.
More Related Videos
09:46Fabrication and Characterization of High-Q Silicon Nitride Membrane Resonators
Published on: August 8, 2025
11:47Characterization of Surface Modifications by White Light Interferometry: Applications in Ion Sputtering, Laser Ablation, and Tribology Experiments
Published on: February 27, 2013