Xylan and xylose decomposition during hot water pre-extraction: A pH-regulated hydrolysis
Xiheng Kang1, Yun-Yan Wang2, Shuangfei Wang1
1School of Light Industry and Food Engineering, Guangxi University, Nanning 530004, PR China; Guangxi Key Laboratory of Clean Pulp & Papermaking and Pollution Control, Nanning 530004, PR China.
Abstract:
One of the key issues in the development of biofuels using lignocellulosic feedstocks is to increase the yield of fermented sugar, and simultaneously decrease the generation of fermentation inhibitors. Therefore, it is essential to understand the degradation mechanism of xylan during hot-water pretreatment. We analyzed the hydrothermal degradation products of xylan and xylose under different conditions. Results showed that furfural and formic acid formed from xylose reached a maximum value of 32.56 % and 35.14 %, respectively. By increasing the initial pH of the xylan solution, the furfural concentration can be reduced effectively to 2% and the formation of formic acid was preferred under alkaline conditions. On this basis, we proposed a new hydrothermal degradation pathway of xylan in alkaline solution. The in-depth understanding of xlyan degradation during hot water pre-treatment will be beneficial for improving the efficiency of biofuel production.
More Related Videos
11:49Sequencing of Plant Wall Heteroxylans Using Enzymic, Chemical Methylation and Physical Mass Spectrometry, Nuclear Magnetic Resonance Techniques
Published on: March 24, 2016
10:18Extraction of Lignin with High β-O-4 Content by Mild Ethanol Extraction and Its Effect on the Depolymerization Yield
Published on: January 7, 2019