Related Experiment Video
Updated: Nov 21, 2025

Scale-up Chemical Synthesis of Thermally-activated Delayed Fluorescence Emitters Based on the Dibenzothiophene-S,S-Dioxide Core
Published on: October 24, 2017
Rigid Polyimides with Thermally Activated Delayed Fluorescence for Polymer Light-Emitting Diodes with High External
Yubo Long1, Xiaojie Chen1, Huiyan Wu1
1Department PCFM Lab and GD HPPC Lab, Guangdong Engineering Technology Research Center for High-performance Organic and Polymer Photoelectric Functional Films, State Key Laboratory of Optoelectronic Material and Technologies, School of Chemistry, Sun Yat-sen University, Guangzhou, 510275, China.
Abstract:
A series of rigid nonconjugated polyimide (PI)-based thermally activated delayed fluorescence (TADF) polymers were reported for the first time, based on a "TADF-Linker-Host" strategy. Among of which, the TADF unit contains a typical TADF luminous core structure, the "Host" unit exhibits effective conjugation length that endows polyimide with high triplet energy, and the "Linker" unit has an aliphatic ring structure to improve solubility and inhibits intramolecular charge transfer effect. All the TADF polymers exhibit high thermal stability (Tg >308.7 °C) and refractive index (1.76-1.79). Remarkably, highly-efficient polymer light-emitting diodes (PLEDs) based on the polymers are successfully realized, leading to a maximal external quantum efficiency of 21.0 % along with low efficiency roll-off. Such outstanding efficiency is amongst the state-of-the-art performance of nonconjugated PLEDs, confirming the effectiveness of structural design strategy, providing helpful and valuable guidance on the development of highly-efficient fluorescent polymer materials and PLEDs.
More Related Videos
Related Concept Videos
Photoluminescence: Applications
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...