The Influence of Starch Origin on the Properties of Starch Films: Packaging Performance
Zuzanna Żołek-Tryznowska1, Alicja Kałuża1
1Division of Printing Technologies, Mechanics and Printing Institute, Faculty of Production Engineering, Warsaw University of Technology, Konwiktorska 2, 00-217 Warsaw, Poland.
Abstract:
Starch films can be used as materials for food packaging purposes. The goal of this study is to compare how the starch origin influence the selected starch film properties. The films were made from various starches such as that from maize, potato, oat, rice, and tapioca using 50%w of glycerine as a plasticizer. The obtained starch-based films were made using the well-known casting method from a starch solution in water. The properties of the films that were evaluated were tensile strength, water vapour transition rate, moisture content, wettability, and their surface free energy. Surface free energy (SFE) and its polar and dispersive components were calculated using the Owens-Wendt-Rabel-Kaelbe approach. The values of SFE in the range of 51.64 to 70.81 mJ∙m-2 for the oat starch-based film and the maize starch-based film. The films revealed worse mechanical properties than those of conventional plastics for packaging purposes. The results indicated that the poorest tensile strength was exhibited by the starch-based films made from oat (0.36 MPa) and tapioca (0.78 MPa) and the greatest tensile strength (1.49 MPa) from potato.
Related Concept Videos
Factors Influencing Drug Absorption: Pharmaceutical Parameters
Polymer Classification: Stereospecificity
Factors Affecting Dissolution: Drug Permeability, Stability and Stereochemistry
Chemistry of Carbohydrates
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...