Incorporation of Wheat Straw Ash as Partial Sand Replacement for Production of Eco-Friendly Concrete

Shazim Ali Memon1, Usman Javed2, Muhammad Haris3

  • 1Department of Civil and Environmental Engineering, School of Engineering and Digital Sciences, Nazarbayev University, Astana 010000, Republic of Kazakhstan.

Related Concept Videos

Design Example: Sustainability in Concrete Building01:26

Design Example: Sustainability in Concrete Building

As the construction industry moves towards more eco-friendly practices, concrete's adaptability and its ability to incorporate sustainable features make it a key material in the drive towards greener building solutions.
There are multiple approaches to achieve sustainability in a commercial concrete building. For instance, construct a concrete parking area under the building, utilizing pervious concrete paver blocks in open areas to facilitate rainwater collection through an underground...
272
Additives and Fillers in Concrete01:29

Additives and Fillers in Concrete

Additives and fillers are integral to enhancing the properties of concrete. Pozzolans and blast-furnace slag are additives or admixtures due to their reactions with calcium hydroxide released during cement hydration. Fillers, which are finely ground and similar in fineness to Portland cement, improve concrete attributes such as workability density, and reduce capillary bleeding or cracking. Some fillers possess hydraulic properties or participate in benign reactions within the cement paste.
The...
177
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
145
Fiber Reinforced Concrete01:22

Fiber Reinforced Concrete

Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
181
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
339
Abrasion Resistance of Concrete01:23

Abrasion Resistance of Concrete

Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
302