Related Experiment Video
Updated: Oct 27, 2025

Fused Filament Fabrication FFF of Metal-Ceramic Components
Published on: January 11, 2019
Synthesis and Characterization of Mechanical Properties and Wire Cut EDM Process Parameters Analysis in AZ61
Thanikodi Sathish1, Vinayagam Mohanavel2, Khalid Ansari3
1Department of Mechanical Engineering, Saveetha School of Engineering, Saveetha Institute of Medical and Technical Sciences (SIMATS), Chennai 602105, India.
Abstract:
Wire Cut Electric Discharge Machining (WCEDM) is a novel method for machining different materials with application of electrical energy by the movement of wire electrode. For this work, an AZ61 magnesium alloy with reinforcement of boron carbide and silicon carbide in different percentage levels was used and a plate was formed through stir casting technique. The process parameters of the stir casting process are namely reinforcement %, stirring speed, time of stirring, and process temperature. The specimens were removed from the casted AZ61 magnesium alloy composites through the Wire Cut Electric Discharge Machining (WCEDM) process, the material removal rate and surface roughness vales were carried out creatively. L 16 orthogonal array (OA) was used for this work to find the material removal rate (MRR) and surface roughness. The process parameters of WCEDM are pulse on time (105, 110, 115 and 120 µs), pulse off time (40, 50, 60 and 70 µs), wire feed rate (2, 4, 6 and 8 m/min), and current (3, 6, 9 and 12 Amps). Further, this study aimed to estimate the maximum ultimate tensile strength and micro hardness of the reinforced composites using the Taguchi route.
Related Concept Videos
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in...