Related Experiment Video
Updated: Oct 23, 2025

High-Contrast and Fast Photorheological Switching of a Twist-Bend Nematic Liquid Crystal
Published on: October 31, 2019
Poplar-based thermochromic composites that change colour at 38 °C to 46 °C
Weihua Zou1, Zimu Li2, Zhangheng Wang2
1Central South University of Forestry and Technology, Shaoshan South Road 498, Changsha, 410004, China. weibick@sina.cn.
Abstract:
The red thermochromic dye (R-TD) is the tetradecanoic acid tetradecyl ester (C28H56O2) and methyl red (C15H15N3O2) mixture that has better permeability enabling its infiltration into wood and better thermochromic properties changing its colour at above 30 °C after about 0.5 min. Thicker poplar-based thermochromic composite specimens (R-PTC, thickness: 5.0 mm) were prepared by filling the R-TD into pre-treated poplar veneer (thickness: 5.0 mm) thus allowing better penetration after pre-treatment. After R-TD infiltration, the R-PTC samples were covered by polypropylene wax for preventing R-TD from overflowing from R-PTC under the action of phase-change temperature. This R-PTC, whose colour can change from light-red to dark-red at 38 °C to 46 °C, can recover to light-red at below 38 °C after about 14 h, and the peak of colour change is at about 42 °C. R-PTC will be suitable for materials used in thermochromic furniture that can indicate the surface temperature to potential users, thus allowing assessment of likely scalded pain when used the furniture.
Related Concept Videos
Thermal Sigmatropic Reactions: Overview
Sigmatropic shifts are classified based on an order term [i, j ], where i and j indicate the number of atoms across which each end of the σ bond migrates. Below are examples of a [3,3] sigmatropic shift in...
Thermosensation