Related Experiment Video
Updated: Oct 22, 2025

Author Spotlight: Enhancing Fiber Composite Laminate Quality with the Wet Hand Lay-Up/Vacuum Bag Process
Published on: June 30, 2023
Workability and Flexural Properties of Fibre-Reinforced Geopolymer Using Different Mono and Hybrid Fibres
Jacob Junior1, Ashish Kumer Saha1, Prabir Kumar Sarker1
1School of Civil and Mechanical Engineering, Curtin University, Perth, WA 6102, Australia.
Abstract:
The effects of mono (single type) and hybrid (mixed types) fibres on the workability, compressive strength, flexural strength, and toughness parameters of fly ash geopolymer mortar were studied. The ratio of sand to geopolymer paste of the mortar was 2.75. It was found that workability of mortar decreased more with the use of PP fibres due to its higher dispersion into individual filaments in geopolymer mortar compared to the bundled ARG and PVA fibres. Compressive strength increased by 14% for using 1% steel with 0.5% PP fibres compared to that of the control mixture, which was 48 MPa. However, 25 to 30% decrease of compressive strength was observed in the mortars using the low-modulus fibres. Generally, flexural strength followed the trend of compressive strength. Deflection hardening behaviours in terms of the ASTM C1609 toughness indices, namely I5, I10 and I20 were exhibited by the mortars using 1% steel mono fibres, 0.5% ARG with 0.5% steel and 1% PVA with 0.5% steel hybrid fibres. The toughness indices and residual strength factors of the mortars using the other mono or hybrid fibres at 1 or 1.5% dosage were relatively low. Therefore, multiple cracking and deflection hardening behaviours could be achieved in fly ash geopolymer mortars of high sand to binder ratio by using steel fibres in mono or hybrid forms with ARG and PVA fibres.
Related Concept Videos
Fiber Reinforced Concrete
Workability of Concrete
Concrete's workability is determined by its resistance to internal forces that arise...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Pozzolans
Fly ash is...
Additives and Fillers in Concrete
The...