Performance and Cost-Effectiveness of Short Pitch-Based Carbon Fiber Reinforced Mortar Composite

Md Safiuddin1,2,3, George Abdel-Sayed3, Nataliya Hearn3

  • 1Angelo DelZotto School of Construction Management, George Brown College, 146 Kendal Avenue, Toronto, ON M5T 2T9, Canada.

Related Concept Videos

Fiber Reinforced Concrete01:22

Fiber Reinforced Concrete

Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
171
Accelerated Curing of Concrete01:25

Accelerated Curing of Concrete

Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
287
Mortar Properties01:17

Mortar Properties

Mortar properties encompass a range of characteristics crucial for construction and masonry work, including workability, water retention, bond strength, durability, compressive strength, volume change, and appearance. Workability refers to mortar's ability to be easily applied and manipulated without sagging or falling off surfaces, which is important for efficient masonry unit placement and alignment. Water retention is essential to prevent the mortar from losing moisture too quickly to...
231
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
254
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
183
Impact Strength of Concrete01:21

Impact Strength of Concrete

Impact strength in concrete is a critical measure that reflects the material's capability to endure the forces applied during pile driving and when supporting machinery foundations that experience impulsive loads. It is also essential when handling precast concrete components to prevent accidental damage. The impact strength is assessed by observing the concrete's resistance to repeated impacts and energy absorption capacity. A key indicator of significant damage to concrete is when it...