Analysis of Bubble Growth in Supercritical CO2 Extrusion Foaming Polyethylene Terephthalate Process Based on Dynamic
Shun Yao1, Yichong Chen1, Yijie Ling1
1Shanghai Key Laboratory of Multiphase Materials Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China.
Abstract:
Bubble growth in the polymer extrusion foaming process occurs under a dynamic melt flow. For non-Newtonian fluids, this work successfully coupled the dynamic melt flow simulation with the bubble growth model to realize bubble growth predictions in an extrusion flow. The initial thermophysical properties and dynamic rheological property distribution at the cross section of the die exit were calculated based on the finite element method. It was found that dynamic rheological properties provided a necessary solution for predicting bubble growth during the supercritical CO2 polyethylene terephthalate (PET) extrusion foaming process. The introduction of initial melt stress could effectively inhibit the rapid growth of bubbles and reduce the stable size of bubbles. However, the initial melt stress was ignored in previous work involving bubble growth predictions because it was not available. The simulation results based on the above theoretical model were consistent with the evolution trends of cell morphology and agreed well with the actual experimental results.
More Related Videos
07:10Production of Membrane-Filtered Phase-Shift Decafluorobutane Nanodroplets from Preformed Microbubbles
Published on: March 23, 2021
11:08Generation of Size-controlled Poly ethylene Glycol Diacrylate Droplets via Semi-3-Dimensional Flow Focusing Microfluidic Devices
Published on: July 3, 2018
Related Concept Videos
Turbulent Flow: Problem Solving
Temperature is a key factor in CO2 solubility. In this case, the CO2 gas and the liquid are cooled to 20°C. Lower temperatures...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Excess Pressure Inside a Drop and a Bubble
Steady, Laminar Flow in Circular Tubes
Step-Growth Polymerization: Overview
Many natural and synthetic polymers are produced by...