Electrospun Shape-Stabilized Phase Change Materials Based on Photo-Crosslinked Polyethylene Oxide

Giulia Fredi1,2, Parnian Kianfar3, Sara Dalle Vacche3,4

  • 1Department of Industrial Engineering, University of Trento, 38123 Trento, Italy.

Polymers
|September 10, 2021
PubMed

Related Concept Videos

Types of Step-Growth Polymers: Polyesters01:20

Types of Step-Growth Polymers: Polyesters

The introduction of polyesters has brought major development to the textile industry. The wrinkle-free behavior of polyester blends has eliminated the need for starching and ironing clothes.
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
2.4K
Olefin Metathesis Polymerization: Ring-Opening Metathesis Polymerization (ROMP)01:16

Olefin Metathesis Polymerization: Ring-Opening Metathesis Polymerization (ROMP)

Ring-opening metathesis polymerization or ROMP involves strained cycloalkenes as starting materials. The mechanism of ROMP proceeds by reacting cycloalkene with Grubbs catalyst to give metallacyclobutane intermediate which undergoes a ring-opening reaction to form new carbene. The new carbene reacts with another molecule of cycloalkene. Repetition of these steps leads to the formation of an unsaturated open-chain polymer product. All these steps are reversible, however, relieving the ring...
2.8K
Thermal and Photochemical Electrocyclic Reactions: Overview01:26

Thermal and Photochemical Electrocyclic Reactions: Overview

Electrocyclic reactions are reversible reactions. They involve an intramolecular cyclization or ring-opening of a conjugated polyene. Shown below are two examples of electrocyclic reactions. In the first reaction, the formation of the cyclic product is favored. In contrast, in the second reaction, ring-opening is favored due to the high ring strain associated with cyclobutene formation.
2.5K