Effect of Short Fibres in the Mechanical Properties of Geopolymer Mortar Containing Oil-Contaminated Sand
Rajab Abousnina1, Haifa Ibrahim Alsalmi2, Allan Manalo2
1School of Engineering, Faculty of Science and Engineering, Macquarie University, Sydney, NSW 2109, Australia.
Abstract:
Sand contaminated with crude oil is becoming a major environmental issue around the world, while at the same time, fly ash generated by coal-fired power stations is having a detrimental effect on the environment. Previous studies showed that combining these two waste materials can result in an environmentally sustainable geopolymer concrete. Incorporating sand contaminated with crude oil up to a certain level (4% by weight) can improve the mechanical properties of the produced geopolymer concrete but beyond this level can have a detrimental effect on its compressive strength. To overcome this challenge, this study introduces short fibres to enhance the mechanical properties of geopolymer mortar containing fine sand contaminated with 6% by weight of light crude oil. Four types of short fibres, consisting of twisted polypropylene (PP) fibres, straight PP fibres, short glass fibres and steel fibres in different dosages (0.1, 0.2, 0.3, 0.4 and 0.5% by volume of geopolymer mortar) are considered. The optimum strength was obtained when straight PP fibres were used wherein increases of up to 39% and 74% of the compressive and tensile strength, respectively, of the geopolymer mortar were achieved. Moreover, a fibre dosage of 0.5% provided the highest enhancement in the mechanical properties of the geopolymer mortar with 6% crude oil contamination. This result indicates that the reduction in strength of geopolymer due to the addition of sand with 6% crude oil contamination can be regained by using short fibres, making this new material from wastes suitable for building and construction applications.
More Related Videos
11:07Preparation of Aligned Steel Fiber Reinforced Cementitious Composite and Its Flexural Behavior
Published on: June 27, 2018
12:07Fabricating Degradable Thermoresponsive Hydrogels on Multiple Length Scales via Reactive Extrusion, Microfluidics, Self-assembly, and Electrospinning
Published on: April 16, 2018
Related Concept Videos
Deleterious Substances in Aggregate
Another type of impurity is clay and fine material that...
Mortar Properties
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Pore Size Distribution
Adequate...
Porosity in Cement Paste
The balance of water to cement in the mix is...
Pozzolans
Fly ash is...