Ice needles weave patterns of stones in freezing landscapes

Anyuan Li1,2, Norikazu Matsuoka2, Fujun Niu3,4

  • 1Key Laboratory of Rock Mechanics and Geohazards of Zhejiang Province, College of Civil Engineering, Shaoxing University, 312000 Shaoxing, China.

Related Concept Videos

Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
182
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
141
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
163
Stone Masonry01:29

Stone Masonry

Stone masonry is a construction technique that uses individual stones to build structures and can be categorized into two main types: rubble and ashlar. Rubble masonry uses uneven, naturally shaped stones such as river rocks or fragments from quarries. This method often requires the mason to select and possibly shape each stone to fit the designated space, ensuring a proper build, even with irregular stone sizes and shapes. Ashlar masonry, on the other hand, employs uniformly cut stones that...
225
Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units...
153
Phase Transitions: Melting and Freezing02:39

Phase Transitions: Melting and Freezing

Heating a crystalline solid increases the average energy of its atoms, molecules, or ions, and the solid gets hotter. At some point, the added energy becomes large enough to partially overcome the forces holding the molecules or ions of the solid in their fixed positions, and the solid begins the process of transitioning to the liquid state or melting. At this point, the temperature of the solid stops rising, despite the continual input of heat, and it remains constant until all of the solid is...