Biaxial Flexural Strength of High-Translucence Monolithic Ceramics upon Various Thicknesses
Niwut Juntavee1, Apa Juntavee2, Sirintana Phetpanompond3
1Department of Prosthodontics, Faculty of Dentistry, Khon Kaen University, Khon Kaen 40002, Thailand.
Introduction:
High-translucence ceramics have been used increasingly. This study evaluated the biaxial flexural strength of different ceramics as a result of varying thicknesses.
Materials And Methods:
Circular discs with varied thickness of 0.4, 0.6, 0.8, 1.0, 1.2, 1.4, 1.6, 1.8, and 2.0 mm were prepared from high-translucence yttria-partially stabilized zirconia (HTY-PSZ); Bruxzir® Anterior (Bc), and zirconia-reinforced lithium silicate (ZLS) including Celtra® DUO (Cc) and VITA Suprinity® (Vc) (n = 15 discs/group). Biaxial flexural strength (σ) was evaluated utilizing piston-on-three-balls in a testing machine at a speed of 0.5 mm/min. A scanning electron microscope (SEM) was used to determine the microscopic structure. ANOVA and multiple comparisons were analyzed for significant differences (a = 0.05).
Results:
The mean ± sd value of σ (MPa) for thickness 0.4, 0.6, 0.8, 1.0, 1.2, 1.4, 1.6, 1.8, and 2.0 mm was 672.66 ± 107.54, 655.93 ± 93.98, 589.01 ± 63.63, 624.89 ± 87.08, 618.82 ± 83.36, 672.64 ± 84.61, 659.81 ± 122.89, 632.79 ± 92.54, and 657.86 ± 73.17, for Bc; 477.64 ± 88.23, 496.39 ± 86.36, 461.56 ± 57.00, 450.26 ± 86.60, 468.28 ± 83.65, 472.45 ± 53.63, 453.05 ± 72.50, 462.67 ± 47.57, and 535.28 ± 84.33, for Cc; and 500.97 ± 76.36, 506.70 ± 87.76, 557.82 ± 62.78, 543.76 ± 87.29, 507.53 ± 86.09, 502.46 ± 64.75, 557.70 ± 80.91, 527.04 ± 80.78, and 499.88 ± 57.35, for Vc. A significant difference in flexural strength was indicated among groups (p < 0.05). Bc was significantly stronger than Cc and Vc (p < 0.05). Varying thickness did not have a significant influence on strength (p > 0.05). SEM revealed a tight arrangement of crystals for Bc and needle-like crystals diffusing in glass for Vc and Cc.
Conclusion:
Flexural strength of ceramics varied among types, but each retained strength equitably with varying thickness. HTY-PSZ was stronger than ZLS, but each was equally strong for thickness in the range of 0.4-2.0 mm.
Related Concept Videos
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to...
Normal Strain under Axial Loading
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Thin-Walled Hollow Shafts
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...