Abstract:
The formation of ice hangings on the surfaces of concrete tunnel linings and sloped rock masses in cold regions endangers railroad and highway traffic. However, an inexpensive anti-icing material that meets both performance and cost requirements has not yet been developed for application in tunnel and slope engineering infrastructures in cold regions. Most current advanced anti-icing materials are expensive, and fabrication and spraying are both cumbersome, which limits their widespread application to tunnel and slope engineering. Because concrete is a widely used construction material owing to its excellent mechanical properties and low cost, we developed an inexpensive, environmentally friendly anti-icing concrete material (AICM). The AICM can be easily fabricated and sprayed onto the surfaces of large-area concrete or rock substrates and exhibits excellent superhydrophobicity (CA: 151°, SA: 6.7°), surface robustness, water resistance, chemical durability, good anti-icing, easy deicing (deicing stress: 0.06 MPa), and excellent long-term durability in freeze-thaw cycles in low-temperature environments. In addition, a novel fractal theory-based model of ice adhesion shear stress was developed and revealed the mechanism through which an AICM with a composite micro/nanostructure easily deices. The AICM has good application prospects and serves as an important guide for mitigating the formation of ice hangings in tunnel and slope engineering infrastructures in cold regions.
Related Concept Videos
Cold Weather Concreting
To counteract the negative impacts of cold weather, ensuring...
Frost Resistant Concrete
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
Frost Action on Concrete
This freeze-thaw cycle primarily causes surface scaling, where...
Mass Concreting
To reduce the risk of such cracking, the concrete mix may incorporate low-heat cement and pozzolans to reduce the temperature rise. Pre-cooled angular aggregates and water-reducing admixtures...
Design Example: Managing Concrete Workability
Masonry in Cold and Hot Weather Conditions