Diagonal Tensile Test on Masonry Panels Strengthened with Textile-Reinforced Mortar
Dragoș Ungureanu1, Nicolae Țăranu1,2, Dan Alexandru Ghiga1
1Faculty of Civil Engineering and Building Services, "Gheorghe Asachi" Technical University of Iaşi, 43 Mangeron Blvd., 700050 Iaşi, Romania.
Abstract:
This study presents the results of an experimental and numerical program carried out on unreinforced masonry panels strengthened by textile-reinforced mortar (TRM) plastering. For this purpose, five panels were constructed, instrumented and tested in diagonal shear mode. Two panels were tested as reference. The first reference panel was left unstrengthened, while the second one was strengthened by a traditional self-supporting cement mortar matrix reinforced with steel meshes. The remaining three panels were strengthened by TRM plastering applied on one or both faces and connected with transversal composite anchors. The numerical and the experimental results evidenced a good effectiveness of the TRM systems, especially when applied on both panel facings.
Related Concept Videos
Reinforced Brick Masonry
To fortify brick walls...
Posttensioned Masonry Walls
Post-tensioned masonry walls use high-strength steel rods or flexible tendons to enhance the strength and efficiency of masonry structures. These elements are securely anchored to the foundation and extend vertically either within the cores of the masonry units or between the masonry wythes. The construction process involves building the wall with these tensioning elements in place and allowing the mortar to fully cure.
Following the curing process, the tensioning begins. Steel rods are...
Masonry
The process of building with masonry is hands-on and can be executed with basic tools....
Mortar Properties
Mortar Joint Deterioration in Masonry
The...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...