A Methodology to Evaluate Long Term Durability of Dam Concrete Due to Calcium Leaching through Microscopic Tests and

Ding Nie1, Haoyu Wang2, Pengfei Li2

  • 1State Key Laboratory of Simulation and Regulation of Water Cycle in River Basin, China Institute of Water Resources and Hydropower Research, Beijing 100038, China.

Related Concept Videos

Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
207
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
526
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
232
Sulfate Attack on Concrete01:29

Sulfate Attack on Concrete

Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...
334
Soundness of Cement01:17

Soundness of Cement

The soundness of cement refers to the ability of cement paste to retain its volume after setting. Unsound cement can lead to expansion and structural damage due to the presence of free lime, magnesia, and calcium sulfate. Free lime hydrates very slowly, expanding and causing unsoundness, which is difficult to detect because it intercrystallizes with other compounds. Magnesia also reacts with water, forming crystals that can disrupt the cement's structure. Calcium sulfate can create...
270
Drying Shrinkage01:21

Drying Shrinkage

When hardened concrete is exposed to air with a relative humidity of less than 100 percent, it begins to lose the free water within its capillaries. As this water evaporates, the water initially adsorbed onto the calcium silicate hydrates migrates towards these now empty spaces and eventually evaporates as well. Over time, as more water leaves, the volume of the concrete decreases, a phenomenon known as drying shrinkage.
A portion of this drying shrinkage can be reversed; if the concrete is...
178