Experimental Study on Self Compacting Fibrous Concrete Comprising Magnesium Sulphate Solution Treated Recycled

Parthiban Kathirvel1, Gunasekaran Murali1, Nikolai Ivanovich Vatin2

  • 1School of Civil Engineering, SASTRA Deemed University, Thanjavur 613404, India.

Related Concept Videos

Fiber Reinforced Concrete01:22

Fiber Reinforced Concrete

Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
157
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
213
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
132
Bonding and Strength of Aggregate01:12

Bonding and Strength of Aggregate

The bond between aggregate particles and the cement matrix is significantly influenced by the shape and surface texture of the aggregates. High-strength concretes benefit from a rougher texture, which leads to stronger bonding due to greater adhesion. Angular aggregates with larger surface areas also enhance this bond. The bonding quality, however, is complex to assess as no universally accepted test exists. Good bonding is indicated when a crushed concrete specimen shows some aggregate...
266
Compacting Factor test01:22

Compacting Factor test

The compacting factor test is a method used to assess the workability of concrete. It is  especially suitable for concrete mixes containing aggregates up to one and a half inches in size. This test involves specialized equipment consisting of two truncated cone-shaped hoppers and a cylinder, all with polished interior surfaces to minimize friction.
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
292
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...