Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Smear layer deproteinization with NaOCl and HOCl: Do application/wash-out times affect dentin bonding of one-step
Kittisak Sanon1,2, Takashi Hatayama1, Antonin Tichy1,3
1Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University.
Abstract:
This study investigated the influence of application/wash-out times of sodium hypochlorite (NaOCl) and hypochlorous acid (HOCl) on dentin bond strength of one-step self-etch adhesives (1-SEAs). Human coronal dentin discs with a standardized smear layer were pretreated with 6% NaOCl or 100 ppm HOCl for 5 s, 15 s, or 30 s, and washed out with water for 5 s, 15 s or 30 s with or without the application of Clearfil DC Activator (CDA). No pretreatment was used as a control. The discs were bonded with a 1-SEA (Bond Force II or Clearfil Universal Bond Quick) and microtensile bond strength (µTBS) was measured after 24 h. Pretreatment with NaOCl for 15 s and 30 s significantly decreased µTBS (p<0.05), irrespective of wash-out time. The application of CDA recovered µTBS but did not outperform the control group. Conversely, pretreatment with HOCl for 15 s and 30 s followed by 30 s wash-out time significantly increased µTBS of 1-SEAs (p<0.05), regardless of CDA application.