Variation of Critical Water Pressure for Hydraulic Fracturing in Cement Mortar under Sulfate Attack

Detan Liu1,2, Hongwei Zhang1, Zhenzhong Shen1

  • 1College of Water Conservancy and Hydropower Engineering, Hohai University, Nanjing 210098, China.

Related Concept Videos

Sulfate Attack on Concrete01:29

Sulfate Attack on Concrete

Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...
333
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
203
Acid Attack on Concrete01:21

Acid Attack on Concrete

When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
364
Types of Cement II01:22

Types of Cement II

Portland blast-furnace cement is made by blending Portland cement clinker with granulated blast-furnace slag, which accounts for 25 to 65 percent of the cement's weight. Despite its similarities to ordinary Portland (Type I) cement in terms of fineness and setting times, its early strength is lower, though it achieves comparable strength later on. It's particularly suited for mass concrete structures and marine environments due to its lower heat of hydration and superior sulfate...
183
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
519
Strength and Heat of Hydration01:29

Strength and Heat of Hydration

The hydration of cement is an exothermic reaction in which heat is generated as cement hydrates. This heat of hydration is critical to cement's strength development. The rate at which this heat is generated affects the temperature rise, with a majority of the heat being released early in the hydration process, half within the first three days, and about 75% within the first week.
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...