Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions
Dongxu Ouyang1, Mingyi Chen2, Jiahao Liu3
1State Key Laboratory of Fire Science, University of Science and Technology of China Hefei 230022 China.
Abstract:
A lithium-ion battery (LIB) may experience overcharge or over-discharge when it is used in a battery pack because of capacity variation of different batteries in the pack and the difficulty of maintaining identical state of charge (SOC) of every single battery. A series of experiments were established to investigate the thermal and fire characteristics of a commercial LIB under overcharge/over-discharge failure conditions. According to the results, it is clear that the batteries experienced a clear temperature rise in the overcharge/over-discharge process. The temperature rise worsened and required less time when the battery was overcharged/over-discharged to failure with the increasing charge/discharge rate. Besides, the closer the position to the opening of the battery, the higher the surface temperature. It was demonstrated that LIBs can fail when overcharged/over-discharged to a critical degree regardless of the charge/discharge rate. Under different rates, the final capacities were around a critical value. Finally, there existed an explosion phenomenon in the external heating test of battery failure after overcharge, whereas the fire behaviors of the over-discharged battery were much more moderate.
Related Concept Videos
Batteries and Fuel Cells
Charging Conductors By Induction
Generally, conductors like metals do not allow any excess charge to be present on them. Any excess charge added to metals easily flows away, for example, when a metal is placed on the Earth. This process is called earthing.
However, conductors can be charged by a process called induction. For example, consider charging a...
Electrogravimetric Analysis: Overview
To test the completeness of the...