Design and Preparation of White High-Strength Concrete with Ground Limestone Powder by Means of Response Surface

Jingliang Xia1,2, Changwei Cao3, Zhengwu Jiang1

  • 1Key Laboratory of Advanced Civil Engineering Materials of Ministry of Education, School of Materials Science and Engineering, Tongji University, Shanghai 201804, China.

Related Concept Videos

Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
124
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
193
Fineness of Cement01:15

Fineness of Cement

The fineness of cement directly influences the rate of hydration, as the hydration begins at the surface of the cement particles. In addition to hydration, the fineness of cement is vital for various properties of concrete including workability, gypsum requirement, and long-term behavior. The fineness of cement is represented in terms of the specific surface of cement which is typically measured in square meters per kilogram, with several methods available for this determination.
Direct...
238
Sulfate Attack on Concrete01:29

Sulfate Attack on Concrete

Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...
321
Response Surface Methodology01:16

Response Surface Methodology

Response Surface Methodology (RSM) is a collection of statistical and mathematical techniques used to develop, improve, and optimize processes. It is particularly valuable when many input variables or factors potentially influence a response variable.
The process of RSM involves several key steps:
292
Design Example: Aggregate Gradation01:24

Design Example: Aggregate Gradation

The right type and quality of aggregates are crucial for concrete as they significantly influence its properties, mix proportions, and cost-effectiveness. If different sources are available for sand, the commonly used fine aggregate in concrete, the selection of sand is primarily based on its gradation.
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
154