Abstract:
Two simple methods are proposed to respectively impart external force-free reversible shape memory effect to commercial polyolefins: ultrahigh molecular weight polyethylene (UHMWPE) and polypropylene (PP). The key issues lie in the utilization of the partially entangled molecular chains of UHMWPE and the medium crystalline phases of PP as the reversible internal stress providers. The acquired reversible shape memory effect further proves to be applicable for assisting repeatedly self-healing of wider cracks. Compared to the conventional approaches, which used to introduce cross-linkages into the target materials, the present ones only need physical treatment, so that the valuable thermoplasticity of polyolefins is retained. This work can be regarded as an example of the concept "physically converting instead of chemically modifying" for the preparation of functional polymeric materials based on market available plastics.
Related Concept Videos
Polymer Classification: Architecture
Polymer Classification: Stereospecificity
Free-Radical Chain Reaction and Polymerization of Alkenes
Olefin Metathesis Polymerization: Overview
Ruthenium-based Grubbs catalyst is the most commonly used catalyst for olefin metathesis polymerization. Grubbs catalyst consists...
Plastic Behavior
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...