Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Bond strength of self-adhesive resin cements to a high transparency zirconia crown and dentin
Jeng-Fen Liu1, Chun-Chuan Yang2, Jun-Liang Luo3
1Department of Pediatric and Physically Disabled Dentistry, Tai Chung Veterans General Hospital, Taichung, Taiwan.
Background/Purpose:
The bond strength and durability of highly translucent zirconia ceramics to dentin is still unclear. The purpose of this study was to investigate the effect of various surface treatments on the bond strength of self-adhesive resin cements to high-translucent zirconia crowns and dentin.
Materials And Methods:
A high-transparent zirconia and three self-adhesive resin cements (G-CEM LinkAce (GCL), RelyX U200 (RXU) and TotalCem (TTC)) were used. The zirconia surface was sandblasted with 50 μm alumina particles or coated with an SR Link primer, while a dentin primer (Tetric N-Bond Universal, TBU) was applied to the surface of the dentin. By using three self-adhesive resin cements, zirconia samples were bonded to the dentin surfaces of human teeth. The shear strength of the specimens was measured before and after 10,000-cycle thermocycling or 90-day aging.
Results:
When using GCL to bond with the untreated dentin and various zirconia surfaces, the shear bond strength of the sandblasted (ZSB) and RS Link primer-coated (ZLK) groups was significantly higher than that of the untreated control group (Zc). However, in the case of TBU-treated dentin, the shear strength of the ZSB + LK + DTBU group was significantly higher than that of the other groups. After thermocycling and aging, the shear strength of the ZSB + LK + DTBU group using GCL and RXU cements decreased slightly, while the TTC showed no impact.
Conclusion:
The zirconia surface pretreated by sandblasting and bonding agent, which was sequentially bonded with a primer-treated dentin by using resin cements, can provide excellent shear bond strength and anti-aging performance.
Related Concept Videos
Bonding and Strength of Aggregate
Transition Zone
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Tooth Anatomy
The Crown, Neck, and Root
The visible part of the tooth is referred to as the crown. It's covered by enamel, the hardest substance in the human body. The crown is uniquely shaped for each type of tooth, allowing for different functions such as cutting, tearing, or...