Related Experiment Video
Updated: Sep 6, 2025

Focused Ion Beam Fabrication of LiPON-based Solid-state Lithium-ion Nanobatteries for In Situ Testing
Published on: March 7, 2018
Long-Life Lithium-Metal All-Solid-State Batteries and Stable Li Plating Enabled by In Situ Formation of Li3 PS4 in
Jieru Xu1,2,3,4, Jiuming Li5, Yongxing Li3,4,6
1Key Laboratory for Renewable Energy, Beijing Key Laboratory for New Energy Materials and Devices, Beijing National Laboratory for Condensed Matter Physics, Institute of Physics, Chinese Academy of Sciences, Beijing, 100190, China.
Abstract:
An ultrastable and kinetically favorable interface is constructed between sulfide-poly(ethylene oxide) (PEO) composite solid electrolytes (CSEs) and lithium metal, via in situ formation of a solid electrolyte interphase (SEI) layer containing Li3 PS4 . A specially designed sulfide, lithium polysulfidophosphate (LPS), can distribute uniformly in the PEO matrix via a simple stirring process because of its complete solubility in acetonitrile solvent, which is advantageous for creating a homogeneous SEI layer. The CSE/Li interface with high Li+ transportation capability is stabilized quickly through in situ formation of a Li3 PS4 /Li2 S/LiF layer via the reaction between LPS and lithium metal to inhibit lithium dendrite growth. A Li/Li symmetric cell with the LPS-integrated CSE exhibits constant and small CSE/Li resistance of 10 Ω cm2 during cycling, delivering stable cycling for 3475 h at a current density of 0.2 mA cm-2 and a high critical current density of 0.9 mA cm-2 at 60 °C. Impressive electrochemical performance is also demonstrated for LiFePO4 /CSE/Li all-solid-state batteries with capacity of 127.6 mAh g-1 after 1000 cycles at 1 C.