Mechanical Behavior of Human Cancellous Bone in Alveolar Bone under Uniaxial Compression and Creep Tests

Bin Wu1, Yang Wu1, Mao Liu2,3,4

  • 1College of Mechanical and Electronic Engineering, Nanjing Forestry University, Nanjing 210037, China.

Related Concept Videos

Behavior of Concrete Under Compressive Load01:23

Behavior of Concrete Under Compressive Load

Concrete exhibits specific behaviors under different compressive loads. Understanding this is crucial for understanding its structural integrity. When concrete undergoes uniaxial compression, it tends to develop cracks that run parallel to the direction of the force. These parallel cracks stem from localized tensile stresses that occur perpendicular to the compression direction. Additionally, angled cracks may appear due to the formation of shear planes.
As the concrete specimen fractures under...
254
Normal Strain under Axial Loading01:20

Normal Strain under Axial Loading

Normal strain under axial loading is an important concept in the field of mechanics of materials. Axial loading implies the application of a force along the axis of a material, like a column or bar. This force can either compress or stretch the material. In the context of axial loading, normal strain is the deformation experienced by the material in the direction of the loading force. It's calculated as the change in length divided by the original length of the material. This unitless ratio...
633
Creep in Concrete01:22

Creep in Concrete

Creep refers to the time-dependent increase in strain under a sustained load, excluding other time-dependent deformations associated with shrinkage, swelling, and thermal expansion in concrete. The primary mechanism behind creep involves the loss of physically adsorbed water from the calcium silicate hydrate within the hydrated cement paste. This process is further exacerbated by concrete's non-linear stress-strain relationship, microcrack development in the interfacial transition zone, and...
405